Typical applications include protecting/ containment of low temperature CFL/CFT bulbs, colored/decorating low temp CFL/CFT bulbs, all types of glass products and containers.
Technical Specs
Brands |
N/A Performix® |
Solids Weight |
N/A 37 to 39 % |
Elongation |
N/A 825 % |
Elongation Test Method |
N/A American Society for Testing and Materials (ASTM D-412) |
Tensile |
N/A 3,680 psi |
Tensile Test Method |
N/A American Society for Testing and Materials (ASTM D-412) |
Tear Resistance |
N/A 0.70 |
Tear Resistance Test Method |
N/A American Society for Testing and Materials (ASTM D-1004) |
Freeze Thaw Stability |
N/A Excellent |
Shelf Life |
N/A 1+ years at 77 ºF unopened container |
Finish |
N/A Semi-Gloss |
Abrasion |
N/A Excellent |
Permeability |
N/A Limited |
Temperature Use Range |
N/A 0 to 250 ºF |
Weatherability |
N/A Excellent 7-10 years |
Weatherability Test Method |
N/A American Society for Testing and Materials (ASTM G-53) |
Chemical Resistance |
N/A
Petroleum: Excellent Acid, Alkaline: Good Alcohol, Ketone, Chlorinated Solvent: Limited |
Alternative Products |
N/A Contact Technical Service. |
Surface Preparations
|
N/A
MIX WELL BEFORE USE. |
Spraying
|
N/A Pressure pot/conventional sprayers may be used. Gently mix before spraying. Apply wet, overlapping coats, holding gun 6"-12" from surface, using a 4"- 6" pattern. Allow to completely dry before applying additional coats to desired thickness. |
Recommended Equipment and Settings
|
N/A
Gun: Binks® model 2100 |
Dipping
|
N/A Gently mix before each use. Do not introduce air bubbles. Insert item 1" every 5 seconds. Remove at same rate. Allow to completely dry before applying additional coats to desired thickness. |
Brush/Roller
|
N/A Gently mix before each use. Apply wet overlapping coats using a foam brush, pad or roller. Allow to completely dry before applying additional coats to desired thickness. |
Hints
|
N/A For storage or dip tank containers, use only poly or galvanized steel. A dry film thickness of 2-3 mils is recommended for most applications. To speed drying, mild heat (95ºF-130ºF) and air flow may be used. To cross link bake coated product between 130-350ºF for upto 30 minutes. Do not stack or store parts in contact with each other if not fully cured. Avoid excessive air movement, heat or humidity. Always use proper ventilation and protection. |
Note
|
N/A
For Industrial Use Only. |